2010年7月4日星期日

Increase In fineness

  1. The rate of hydration increases . This leads to both a higher rate of strength gain and higher rate of evolution of heat .
  2. Decrease the amount of bleeding , but the amount of water required for workability for non -air entrained concrete is increases , which results in increased drying shringkage result in surface cracking.
  3. Reduce the durability of concrete to freeze-thraw cycles
  4. Requires a greater amount of gymsum for proper set control , owing to the increased aailabitlity of C3S for reaction
  5. Increase in production cost
  6. Quality can easliy be detrimental when expose to air .
  7. Increases in reaction with some aggregates = aggregates degradation